undefined
+
  • undefined

TPEE Drive Belt Material

A high-performance TPEE material specifically developed for drive belts in automotive engine accessory systems, industrial equipment, and office automation devices.

  • Product Description
  • 概要
  • Item

    Description

    Product Name

    High-Strength Thermoplastic Polyester Elastomer for Synchronous/Poly-V Belts

    Product Description

    A high-performance TPEE material specifically developed for drive belts in automotive engine accessory systems, industrial equipment, and office automation devices.

    Key Characteristics

    1. Extremely High Tensile Strength & Modulus: Provides powerful load-bearing capacity, preventing belt breakage under high-speed and high-load conditions.
    2. Very Low Dynamic Elongation & Excellent Creep Resistance: Ensures precise synchronous power transmission, prevents slippage and ratio inaccuracy, with minimal elongation over time.
    3. Exceptional Flex Fatigue & Crack Growth Resistance: Maintains structural integrity after millions of flexing cycles over pulleys, resulting in long service life.

    Main Applications

    Automotive engine timing belts, accessory serpentine belts, industrial synchronous belts, printer/copier drive belts, treadmill belts for fitness equipment.

    Processing Method

    Precision Extrusion (Primary), often over reinforced cord (e.g., fiberglass, aramid), or molded into tooth profiles.

    Key Certs/Standards

    Compliant with automotive OEM material specifications (e.g., GMW, VW, Ford), industrial standards (e.g., RMA, ISO), and environmental requirements (RoHS, REACH).

    Color

    Typically black or dark colors.

    Appearance

    Uniform pellets or custom-cut granules.

    Packaging

    20/25 kg/bag

    Physical Properties (Typical Example)

    Property

    Typical Value/Example

    Unit

    Test Standard

    Specific Gravity

    1.20 - 1.30

    g/cm³

    ASTM D792

    Hardness (Shore D)

    55D - 65D (common)

    Shore D

    ASTM D2240

    Tensile Strength

    ≥ 40

    MPa

    ASTM D412

    Stress at 100% Elongation

    ≥ 15

    MPa

    ASTM D412

    Elongation at Break

    300 - 450

    %

    ASTM D412

    Compression Set

    ≤ 40

    %

    ASTM D395

    Tensile Strength Retention after Heat Aging

    ≥ 80%

    --

    ASTM D573

    Processing Reference Thorough drying is MANDATORY: Recommend 4-6 hours at 120-125°C to achieve moisture content <0.02%. Melt Temperature: 210-240°C; precise control of all extrusion zone temperatures is required.

    Key Notes

    Extremely Stringent Drying & Cleanliness: Any trace moisture causes hydrolytic degradation of TPEE during high-temperature extrusion, severely reducing molecular weight, tensile strength, and fatigue life, which is a primary cause of premature belt failure.